Hex Nuts, Superalloy (Inconel, Hastelloy, Alloy 20) (a286ora-286)
Finished Hex nuts are hexagonal, internally threaded fasteners, mated with bolts, studs, screws, and other externally threaded products. The purpose of a hex nut is to ensure that the bolt, etc., stays in place. Hex nuts of standard thickness are called finished hex nuts.
4 results, (click on any line for more information)
Buy Hex Nuts from one of our FCH Network Members | ||||||||
---|---|---|---|---|---|---|---|---|
Supplier | Loc | Type | Material | Finish | Size | Description | Qty | |
MTP | CA | Finished Hex Nut | Superalloy (Inconel, Hastelloy, Alloy 20) | Plain | 1/4-20 | 1/4-20 a286 age hardened hex nuts A286959025001 | stock |
|
MMCC | IL | Finished Hex Nut | Superalloy (Inconel, Hastelloy, Alloy 20) | Plain | M4-0.70 | m4x.7 s c nut a286 din 867g | inquire |
|
CNB | IL | Finished Hex Nut | Superalloy (Inconel, Hastelloy, Alloy 20) | Passivated | 5/8-11 | hex nut a-286 heat treated and per print less note 4 | 19 |
|
Hewes | NY | Finished Hex Nut | Superalloy (Inconel, Hastelloy, Alloy 20) | Silver | slf lkg nutnasm21043-4cres a286 silver plate | 58 |
|