Supplier | Loc | Type | Material | Finish | Size | Description | Qty | |
Komar | IL | Springs (Compression) | Superalloy (Inconel, Hastelloy, Alloy 20) | .276/.256d x.701lgcompression spring(.029d)17-7ph | 5650 |
| ||
Komar | IL | Springs (Compression) | Superalloy (Inconel, Hastelloy, Alloy 20) | .249 | .249/.241d x1.860lg compression spring(.026)17-7ph | 750 |
| |
Komar | IL | Springs (Compression) | Superalloy (Inconel, Hastelloy, Alloy 20) | .126 | .126 maxd x.215lg compression spring(.014d)17-7ph | 10730 |
| |
Exim | S'pore | Springs (Compression) | Superalloy (Inconel, Hastelloy, Alloy 20) | M1-17 | crest-to-crest spirawave springcompression circular grain sinusoidal17-7 ph s/s condition ch900 c100-m1-s17 | 2 |
|